Nitrogen substitution method
Welding, as when heating without nitrogen substitution a large amount of the oxide film is formed
on the internal piping.
The oxide film is a caused by clogging EEV, Capillary, oil hole of accumulator and suction hole of oil
pump in compressor.
It prevents normal operation of the compressor.
In order to avoid this problem, Welding should be done after replacing air by nitrogen gas.
When welding plumbing pipe, the work is required.
◆How to work
Oxide scale
Note) should not block the outlet side.
When the internal pressure in pipe is abo
ve the atmospheric pressure, pinhole is o
ccurred and it is a leakage cause.
CAUTION
1. Always use the nitrogen.(not use oxygen, carbon dioxide, and a Chevron gas):
Please use the following nitrogen pressure 0.02 MPa
Oxygen --------- Promotes oxidative degradation of refrigerant oil.
Because it is flammable, it is strictly prohibited to use
Carbon dioxide --- Degrade the drying characteristics of gas
Chevron Gas ---- Toxic gas occurs when exposed to direct flame.
2. Always use a pressure reducing valve.
3. Please do not use commercially available antioxidant.
The residual material seems to be the oxide scale is observed.
In fact, due to the organic acids generated by oxidation of the alcohol contained in the anti-
oxidants, ants nest corrosion occurs. (causes of organic acid ' alcohol + copper + water +
temperature)
Welding Point
Nitrogen gas
Pressure 0.02MPa less
Taping
(Should not
contain air)
Connecting Copper Pipes
Regulator
Auxiliary valve
Installation Manual 13

Hide quick links:

Advertisement

Table of Contents
loading

This manual is also suitable for:

Auuw36gd2Auuw42gd2Luu247hvLuu360hvLuu427hv

Table of Contents

Uploaded: cache9/manual/3420760/Lg-Auuw24gd2.html%3Fpage%3D13.gz